Aluminium 5052 (EN AW-5052 / UNS A95052)

Non-heat-treatable Al–Mg alloy with good corrosion resistance (marine), weldability and medium strength.

Typical temper shown here: H32.

Standards & designations

DesignationReference
AA/UNSAA 5052 / UNS A95052
ENEN AW-5052 (EN 573-3 chemistry; EN 485-2 mechanical)
ASTMB209/B209M (sheet & plate)
ISOAlMg2.5

Mechanical & physical properties

PropertyValue / condition
Temper / ProductH32 (sheet/plate)
Tensile strength Rm215–265 MPa
Yield strength Rp0.2≥ 160 MPa
Elongation A507–11 % (thickness dependent)
Hardness HB~ 60–75
Density≈ 2.68–2.70 g/cm³
Young’s modulus E≈ 70 GPa
Thermal conductivity~ 138 W/m·K

Chemical composition

Weight %

ElementSiFeCuMnMgCrZnOthers (each)Others (total)Al
Min————2.20.15———bal.
Max0.250.400.100.102.80.350.100.050.15bal.