Alloy C-22 (Hastelloy® C-22, UNS N06022)

Ni-Cr-Mo-W corrosion-resistant alloy with superior resistance to localized corrosion vs. C-276 and 625.

Standards & designations

DesignationReference
UNSN06022
Werkstoff Nr.2.4602
ASTMB575 (plate/sheet), B574 (bar), B622 (pipe), B619/B626 (tubing)
ASMESB575, SB574, SB622, SB619/SB626
ISOISO 15156-3 (sour service)
OthersHastelloy® C-22

Mechanical properties

PropertyValue / condition
Yield strength Rp0.2≥ 310 MPa (min, typ. product)
Tensile strength Rm≥ 690 MPa (min)
Elongation≥ 40 % (min)
Hardness—

Chemical composition

Weight %

ElementNiCrMoWFeCoMnSiCPS
Minbal.20.012.52.52.0——————
Maxbal.22.514.53.56.02.50.50.080.0150.020.02

Applications & processing

Applications

chemical processing, sour service, scrubbers, heat exchangers.

Heat treatment

Solution anneal ~ 1120–1175 °C; rapid quench.

Weldability

Very good.