MATERIAL DATASHEET

17-4 PH (UNS S17400 / EN 1.4542)

Precipitation-hardening martensitic stainless steel; high strength after aging (H900–H1150), good corrosion resistance.

Standards & designations

DesignationReference
UNSS17400
Werkstoff Nr.1.4542
ASTMA564 (bar), A705 (forgings), A693 (plate)
ASMESA564, SA705, SA693
EN/ISOEN 10088-3 (1.4542)
OthersX5CrNiCuNb16-4

Mechanical properties

PropertyValue / condition
Yield strength Rp0.2≥ 1000–1310 MPa (aged, condition dependent)
Tensile strength Rm≥ 1070–1310+ MPa
Elongation~ 10–20 %
Hardness~ HRC 28–44 (condition dependent)

Chemical composition

Weight %

ElementCrNiCuNb+TaCMnSiPSFe
Min15.03.03.00.15—————bal.
Max17.55.05.00.450.071.01.00.040.03bal.

Applications & processing

Applications

shafts, fasteners, valve parts, aerospace and energy components.

Heat treatment

Solution treat, then age (e.g., H900, H1025, H1150).

Weldability

Good (match filler).